The bulk density of refractory ceramic fiber refers to the ratio of the weight of ceramic fiber to the overall material. The size of the bulk density is an indicator to determine whether the furnace lining is reasonable. It is an important factor affecting the thermal conductivity.
A. The thermal conductivity of ceramic-fiber products decreases with the increase of the bulk density, but the decreasing range gradually decreases, so that when the density exceeds A certain range, the thermal conductivity no longer decreases, but has a tendency to increase.
B. There is a minimum thermal conductivity and corresponding minimum volume density at different temperatures, and the volume density corresponding to the minimum thermal conductivity increases with the increase of temperature.
It is of great significance to correctly understand and apply the above laws to the application of ceramic fibers. The adiabatic performance of ceramic fibers is mainly based on the adiabatic effect of the sealed air in the pores of products. When the proportion of solid fibers is certain, the larger the porosity is, the smaller the volume density is.
When the bulk density is less than 96Kg/m³, due to the enhanced oscillating convection and radiative heat transfer of the gas in the mixed structure, the thermal conductivity decreases with the bulk density, showing an increasing trend of an exponential function.
When the bulk density is >96Kg/m³, as the bulk density increases, the pores distributed in the fiber are closed, the proportion of micropores increases, the air flow in the pores is restricted, the heat transfer in the fiber decreases (the thermal resistance increases), and at the same time it causes The radiation heat transfer between the walls of the holes is also correspondingly reduced, thereby reducing the thermal conductivity.
When the bulk density increases to a certain range of 240~320Kg/m³, the contact point of the solid fiber increases, so that the fiber itself forms a mark, and the heat transfer weight increases through the bridge. Secondly, the contact point of the solid fiber increases, and the pores affect the heat transfer. The damping effect is weakened, so that the thermal conductivity no longer decreases and has a tendency to increase. Therefore, the porous fiber material has an optimal volume density with the smallest thermal conductivity. For foreign layered ceramic fiber wall linings, the volume density of ceramic fibers on the hot surface is specified as 130~160Kg/m³, and the volume of ceramic fibers on the hot surface of tiled composite furnace lining The density is specified as 200~240Kg/m³.
After the hot surface of the furnace wall, the volume density of fiber products at all levels decreases successively, because at high temperature, the thermal conductivity of ceramic fiber decreases more significantly with the increase of volume density than at low temperature (as shown in the figure). The fiber lining structure with layers in the thickness direction matched according to the density can keep the thermal resistance uniform in the thickness direction of the furnace lining. Under the same thermal resistance conditions, it can save fiber consumption and reduce furnace construction costs.